Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2350 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.62 - 16.2 GPa
1250 - 2350 ksi
Average value: 12.5 GPa Grade Count:17
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Flexural Modulus 6.55 - 16.2 GPa
950 - 2350 ksi
Average value: 12.3 GPa Grade Count:28
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Flexural Modulus 16.2 - 16.2 GPa

@Temperature 115 - 115 °C
2350 - 2350 ksi

@Temperature 239 - 239 °F
Average value: 9.03 GPa Grade Count:1
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
Flexural Modulus 4.12 - 16.2 GPa
597 - 2350 ksi
Average value: 8.50 GPa Grade Count:44
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..