Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.12 GPa @Thickness 3.20 mm |
597 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® HI2152 PBT+GF15% Description: Injection Molding, PBT+GF15%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 4.12 GPa @Thickness 3.20 mm |
597 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® SG5152 PBT+PET+GF15% Description: Injection Molding, PBT+PET+GF15%, Good Surface, High ImpactApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 4.12 GPa @Thickness 3.20 mm |
597 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5151RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Flexural Modulus | 4.12 GPa @Thickness 6.40 mm |
597 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IMG1120 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Flexural Modulus | 4.12 GPa @Thickness 6.40 mm |
597 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IMG1120 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Flexural Modulus | 4.12 - 16.2 GPa | 597 - 2350 ksi | Average value: 8.50 GPa Grade Count:44 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |