Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.14 - 15.5 GPa | 600 - 2250 ksi | Average value: 9.47 GPa Grade Count:34 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 6.30 - 15.5 GPa | 914 - 2250 ksi | Average value: 9.65 GPa Grade Count:44 |