Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.413 GPa | 204.9 ksi | Test specimens were injection molded by ASTM D1897; ASTM D790 |
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent c.. |
|||
Flexural Modulus | 1.413 GPa | 204.9 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
LyondellBasell DEXFLEX® 940 TPO Description: DEXFLEX® 940 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior painted applications. Applications: Bumper fascias, claddings Information provided by .. |
|||
Flexural Modulus | 1.413 GPa | 204.9 ksi | ASTM D790 |
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t.. |
|||
Flexural Modulus | 1.413 GPa | 204.9 ksi | ASTM D790 |
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give .. |
|||
Flexural Modulus | 1.413 GPa | 204.9 ksi | ASTM D790 |
Chevron Phillips K-Resin® KR05 Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Finished products have excellent clarity, good toughness, good s.. |
|||
Flexural Modulus | 1.413 GPa | 204.9 ksi | ASTM D790 |
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Fin.. |
|||
Flexural Modulus | 1.413 GPa | 204.9 ksi | ASTM D790 |
Chevron Phillips K-Resin® BK11 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK11 is an SBC consisting of KR03 grade with a mold release added of easier processing. BK11 molded parts give excellent detail on fast production cycl.. |