Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1.413 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.413 GPa
204.9 ksi
Test specimens were injection molded by ASTM D1897; ASTM D790
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent c..
Flexural Modulus 1.413 GPa
204.9 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
LyondellBasell DEXFLEX® 940 TPO
Description: DEXFLEX® 940 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior painted applications. Applications: Bumper fascias, claddings Information provided by ..
Flexural Modulus 1.413 GPa
204.9 ksi
ASTM D790
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t..
Flexural Modulus 1.413 GPa
204.9 ksi
ASTM D790
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give ..
Flexural Modulus 1.413 GPa
204.9 ksi
ASTM D790
Chevron Phillips K-Resin® KR05 Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Finished products have excellent clarity, good toughness, good s..
Flexural Modulus 1.413 GPa
204.9 ksi
ASTM D790
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Fin..
Flexural Modulus 1.413 GPa
204.9 ksi
ASTM D790
Chevron Phillips K-Resin® BK11 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: BK11 is an SBC consisting of KR03 grade with a mold release added of easier processing. BK11 molded parts give excellent detail on fast production cycl..
Copyright © lookpolymers.com All Rights Reserved