Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.93 GPa | 425 ksi | Tangent; ASTM D790 |
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
PolyOne Nymax™ 1200 A HS Natural A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
PolyOne Nymax™ 600 A Zip 22 Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6 Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
PolyOne Nymax™ 1200 A L Natural Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive.. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Techmer ES HiFill FR® ABS GB10 FR 10% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Techmer ES HiFill® ABS GB10 10% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Techmer ES HiFill® ABS GB15 15% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Techmer ES Luriblend® PP GF20 GL2 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Graphite Powder Lubricant(2%)Features: LubricatedAppearance: BlackInformation provided by TP.. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PKN4766 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High flow. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Techmer ES HiFill® PP GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | 1% Secant; ASTM D790 |
Washington Penn Homopolymer Polypropylene 30% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Techmer ES Luriblend® POM CO GF5 TL5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by WeightAdditive: PTFE Lubricant(5%)Features: Lubricated and CopolymerInformation provided by TP Composites, In.. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | ASTM D790 |
Amco Amalloy® B1044 Polymer Alloy Amco Amalloy B1044 is a proprietary copolymer with exceptional clarity and toughness.Low haze, low melt flow, high tensile & flexural strength.Information provided by Amco Plastic Materials. |
|||
Flexural Modulus | 2.93 GPa | 425 ksi | Tangent; ASTM D790 |
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |