Polymer Property : Flexural Modulus = 19.0985 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.60 - 19.0985 GPa

@Temperature -40.0 - 149 °C
957 - 2770.04 ksi

@Temperature -40.0 - 300 °F
Average value: 10.3 GPa Grade Count:7
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..