Mechanical Properties Metric English Comments
Flexural Modulus 0.238 - 10.4 GPa
34.5 - 1510 ksi
Average value: 2.79 GPa Grade Count:22
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..
Flexural Modulus 8.16 - 10.4 GPa
1180 - 1510 ksi
Average value: 9.12 GPa Grade Count:10
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and ..