Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.9944 GPa | 144.2 ksi | ASTM D790 |
CPC - Vycom CELTEC MARINE™ Expanded Foam PVC Polyvinyl Chloride Celtec Marine is made from rigid expanded foam polyvinyl chloride (PVC) material whose combination of features makes it ideal for wood trim and plywood replacement in boat manufacturing. Its closed .. |
|||
Flexural Modulus | 0.9944 GPa @Thickness 10.0 - 25.0 mm |
144.2 ksi @Thickness 0.394 - 0.984 in |
ASTM D790 |
CPC - Vycom CELTEC® Expanded Rigid foam PVC board Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface.. |