Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR43 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded
  AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Custom Resins Vexel™ E20GF45 FR , 45% Glass Reinforced, Flame Retardant PET
(discontinued **) Description: Vexel™ E20GF45 FR is a 45% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
PolyOne Edgetek® LC-30GF/000 LCP (Liquid Crystal Polymer), 30% Glass Reinforced, Hi-Temp
(discontinued **)< Information provided by PolyOne™ Corporation |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
PolyOne Edgetek® SF-30GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp RFN18SXZ PA 66 LNP LUBRICOMP* RFN18SXZ is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Ameri.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Clariant Renol PA211G50 Nylon 6, 50% Glass Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 13.1 - 13.8 GPa | 1900 - 2000 ksi | |
Bulk Molding Compounds BMC SLC 1000 Glass Reinforced Polyester BMC SLC 1000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. It is V-0 flame arc and track resistant. UL® recognized. This material was formerly known.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry
(discontinued **) Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10 LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti.. |