Custom Resins Vexel™ E20GF45 FR , 45% Glass Reinforced, Flame Retardant PET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Vexel™ E20GF45 FR , 45% Glass Reinforced, Flame Retardant PET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vexel™ E20GF45 FR is a 45% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins.
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 165 MPa
24000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Modulus 13.1 GPa
1900 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
420 °F
ASTM D648