Polymer Property : Flexural Modulus = 12.4795 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.83 - 12.4795 GPa

@Temperature -40.0 - 121 °C
701 - 1810.03 ksi

@Temperature -40.0 - 250 °F
Average value: 6.81 GPa Grade Count:5
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..