Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.20 - 7.20 GPa @Temperature -40.0 - 80.0 °C |
174 - 1040 ksi @Temperature -40.0 - 176 °F |
Average value: 4.55 GPa Grade Count:1 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |