Polymer Property : Flexural Modulus = 1030 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.686 - 7.11 GPa
99.6 - 1030 ksi
Average value: 2.10 GPa Grade Count:299
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Flexural Modulus 4.00 - 7.10 GPa
580 - 1030 ksi
Average value: 5.52 GPa Grade Count:18
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..