Zylog Hipolyene® 8515 TY Thermoplastic Polyolefin & PP Compound

Category Polymer , Thermoplastic , Polyolefin , Polypropylene (PP)
Manufacturer Zylog Plastalloys
Trade Name Hipolyene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zylog Hipolyene® 8515 TY Thermoplastic Polyolefin & PP Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Melt Flow 10 g/10 min
10 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.5 MPa
3840 psi
Elongation at Break 45 %
45 %
Flexural Modulus 1.77 GPa
256 ksi
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in