Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.56 GPa | 226 ksi | 13 mm/min; ASTM D790 |
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Flexural Modulus | 1.56 GPa | 226 ksi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ 697 ASA Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Flexural Modulus | 1.56 GPa | 226 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 1710 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.56 GPa | 226 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked. |
|||
Flexural Modulus | 1.56 GPa | 226 ksi | ASTM Test |
Styrolution Luran® S 797 SE ASA Luran S 797 SE is an extrusion ASA grade with especially high notched impact strength, used for sheet and profile extrusions. The data representable is based on extruded sheet.Information provided .. |
|||
Flexural Modulus | 1.56 GPa | 226 ksi | ISO 178 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, Conditioned Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Flexural Modulus | 1.56 GPa | 226 ksi | ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Modulus | 1.56 GPa | 226 ksi | ISO 178 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, Conditioned Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |