Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.31 - 1.455 GPa | 190 - 211.0 ksi | ASTM D790M |
DSM Somos® 9120 Epoxy Photopolymer
(Unverified Data**) DescriptionDSM Somos® 9120 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p.. |
|||
Flexural Modulus | 1.31 - 1.455 GPa | 190 - 211.0 ksi | UV Postcure; ASTM D790M |
DSM Somos® 9120 The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp.. |