Polymer Property : Flexural Modulus = 1.378 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Polymer Industries Densetec HDPE Cutting Board
Densetec Cutting Board is engineered for durability, low maintenance and safety. Its textured, matte surface safely holds food in place without slipping. The "natural" bright white color is favored ..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Polymer Industries Densetec HDPE Marine Board
Densetec Marine Board is specially formulated to withstand the rigors of harsh outdoor marine environments. It is UV-stabilized to resist damage and retain its beauty, even after years of direct sun..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Polymer Industries Densetec HDPE Partition Board
Polymer Industries Densetec High Density Polyethylene Partition Board is the ideal partition material for a wide variety of commercial applications such as schools, parks, stadiums, office buildings..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Polymer Industries Densetec HDPE Playground Board
The versatile properties of Densetec Playground Board make it virtually vandal resistant. The UV stabilizers added to the material make the colors fade-resistant and the standard properties of the H..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Polymer Industries Densetec HDPE Sheet
Polymer Industry`s Densetec High Density Polyethylene sheet exhibits the properties of high impact strength, abrasion resistance, and low coefficient of friction. The material is also moisture, stai..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Polymer Industries Densetec HDPE Sign Board
Densetec Sign Board is a coextruded thermoplastic sheet with multiple color layers. The material is manufactured by extruding one color on the inside and a contrasting color on the outside. The laye..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Polymer Industries Densetec HDPE Arena Board
Densetec Arena Board is ideal for hockey rink applications including dasher boards, kick plates and official lines. Densetec Arena Board exhibits the properties of high impact strength, abrasion-res..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Chevron Phillips Marlex® HHM 5502-02 LW High Density Ethylene Hexene Copolymer  (discontinued **)
High Density Ethylene Hexene Copolymer with Synthetic AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and mos..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Chevron Phillips Marlex® HHM 5502-02 LD High Density Ethylene Hexene Copolymer with Antistat  (discontinued **
High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergen..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Chevron Phillips Marlex® C590 High Density Polyethylene  (discontinued **)
High Density PolyethyleneData provided by Chevron Phillips Chemical Company, LP.
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Chevron Phillips Marlex® HMN 55180 High Density Polyethylene  (discontinued **)
High Density PolyethyleneCustomer Benefits: This resin is a narrow molecular weight distribution copolymer with easy processing characteristics and excellent toughness properties. This product disp..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Braskem BS 002 HDPE Blow Molding Polyethylene  (discontinued **)
Applications: Bottles for medicines, cleaning products, cosmetics, food products and surface-active agents. Information provided by Braskem
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of products. Has exce..
Flexural Modulus 1.378 GPa
199.9 ksi
tangent; chs 0.05 in/min; ASTM D790
Diamond Polymers Centrex® 485 Sheet Extrusion Grade
Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it..
Flexural Modulus 1.378 GPa
199.9 ksi
chs 1.3 mm/min; 1% secant; ASTM D790
Diamond Polymers NPP25-0604 Impact Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 1.378 GPa
199.9 ksi
chs 0.05 in/min; ASTM D790
Diamond Polymers NPP50-0355 High Density Polyethylene Blow Molding/Extrusion Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 1.378 GPa
199.9 ksi
0.5"/min crosshead speed; ASTM D790
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat
High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of product..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Polymer Industries Densetec HDPE TredSafe Board
Designed specifically for the Playground and Marine industries, TredSafe incorporates the latest available technologies to produce a non-skid surface ideal for all type of flooring applications.Info..
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Chevron Phillips Marlex® HHM 5502-01 ST High Density Ethylene Hexene Copolymer
High Density Ethylene Hexene CopolymerSag Upper Limit: 18 cm, Lower Limit: 13 cm; 2 ft. X 4ft. X 125 mil thick blank heated to forming temperature.Data provided by Chevron Phillips Chemical Company..