Polymer Industries Densetec HDPE Sheet

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polymer Industries
Trade Name Densetec
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymer Industries Densetec HDPE Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymer Industry`s Densetec High Density Polyethylene sheet exhibits the properties of high impact strength, abrasion resistance, and low coefficient of friction. The material is also moisture, stain and odor resistant, and is FDA approved to be used in the food processing industry. The material`s durability makes it ideally suited for a variety of applications such as water tanks, chute linings and numerous industrial uses.Information provided by Polymer Industries.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 35 hour
35 hour
CO-630; Condition B; ASTM D1693
45 hour
45 hour
CO-630; Condition A; ASTM D1693
Melt Index of Compound 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
2in (50mm) per min.; ASTM D638 Type 4
Elongation at Break >= 600 %
>= 600 %
2in (50mm) per min.; ASTM D638 Type 4
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Brittleness Temperature <= -84.0 °C
<= -119 °F
ASTM D746
Flammability, UL94 HB
HB