Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.990 GPa | 144 ksi | 1% Secant; ASTM D790 |
Flint Hills P5L2Z-038 Random Copolymer Polypropylene Random copolymer, USP Class VI certified, and FDA compliant.Features: Hydrotalcite.Applications: Injection molding: extrusion blow molding and hot fill applications.Former Huntsman polypropylene pro.. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MX12407C PP LNP* STAT-KON* MX12407C is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific) LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | ASTM D790 |
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, MDI-based 2-Component Liquid System 0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C.. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Flexural Modulus | 0.990 GPa | 144 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |