Material Notes:
Random copolymer, USP Class VI certified, and FDA compliant.Features: Hydrotalcite.Applications: Injection molding: extrusion blow molding and hot fill applications.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 0.990 GPa
144 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
23° C; ASTM D256
Gardner Impact 29.0 J
21.4 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ASTM D648