Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.880 GPa | 128 ksi | ASTM D790 |
Kostat BK-STAT P048BK PP Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 7746 A HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GP 100 BK HDPE The resin GP 100 BK is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal tec.. |
|||
Flexural Modulus | 0.880 - 1.37 GPa | 128 - 199 ksi | ASTM D790 |
Zeus EFEP Tubing |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**) Toughened Polyamide 6Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | SAE J949 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | ISO 178 |
Arkema Group OREVAC® CA 100 Grafted Maleic Anhydride Polypropylene OREVAC® CA 100 is a chemically functionalized polypropylene with a high content of maleic anhydride. Grafting on polypropylene backbone is achieved with a processing technology which allows to opti.. |