Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.883 GPa | 128 ksi | ASTM D790 |
Hyosung Topilene C600MU PP C600MU Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 0.883 GPa | 128 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN170SA General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 0.883 GPa | 128 ksi | ASTM D790 |
LG Chemical SEETEC PH150 HDPE Blown Film Grade Features: Characteristics : Excellent weather resistance & Environmental stress cracking resistanceAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 20.. |
|||
Flexural Modulus | 0.883 GPa | 128 ksi | ASTM D760 |
LG Chemical SEETEC R3410 Polypropylene Random Copolymer Features: Seetec R3410 is a polypropylene-ethylene random copolymer designed for the production of expandable PP and films. It has the good clarity due to the appropriate content of ethylene and off.. |
|||
Flexural Modulus | 0.883 GPa | 128 ksi | ASTM D760 |
LG Chemical SEETEC R3420 Polypropylene, Random Copolymer Features: Seetec R3420 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance.. |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | ASTM D790 |
Kostat BK-STAT P048BK PP Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 7746 A HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GP 100 BK HDPE The resin GP 100 BK is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal tec.. |
|||
Flexural Modulus | 0.883 GPa | 128 ksi | ASTM D790 |
SK Chemicals SKYPEL G182D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Flexural Modulus | 0.880 - 1.37 GPa | 128 - 199 ksi | ASTM D790 |
Zeus EFEP Tubing |
|||
Flexural Modulus | 0.882 GPa | 128 ksi | ASTM D790 |
Toyobo PELPRENE™ S9001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON RP-4040 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**) Toughened Polyamide 6Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | SAE J949 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.880 GPa | 128 ksi | ISO 178 |
Arkema Group OREVAC® CA 100 Grafted Maleic Anhydride Polypropylene OREVAC® CA 100 is a chemically functionalized polypropylene with a high content of maleic anhydride. Grafting on polypropylene backbone is achieved with a processing technology which allows to opti.. |
|||
Flexural Modulus | 0.882 GPa | 128 ksi | ASTM D790 |
Asahi Glass Fluon® C-88AXP ETFE Fluororesin A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |