Material Notes:
The resin GP 100 BK is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal technology, has excellent mechanical properties and very high stress cracking resistance and resistance to internal pressure.Applications:Pressure pipes for gas distribution
Physical Properties Metric English Comments
Density 0.960 - 0.962 g/cc
0.0347 - 0.0348 lb/in³
ASTM D792-00
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
ASTM D1693-01
Melt Flow 6.1 - 7.5 g/10 min
6.1 - 7.5 g/10 min
ASTM D1238-04
0.16 - 0.22 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.16 - 0.22 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238-04
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.0 MPa
1450 psi
ISO 9080-03
Flexural Modulus 0.880 GPa
128 ksi
2% secant; ASTM D790-02
Izod Impact, Notched 2.75 J/cm
5.15 ft-lb/in
ASTM D256-03
Descriptive Properties Value Comments
Slow Crack Growth (h) >165
Copyright © lookpolymers.com All Rights Reserved