Flexural Modulus 0.280 GPa
40.6 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer
LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant.
Flexural Modulus 0.280 GPa
40.6 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific)
LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications.
Flexural Modulus 0.280 GPa

@Thickness 19.0 mm
40.6 ksi

@Thickness 0.750 in
ASTM D790
3A Composites Core Materials AIREX® PXc.245 Fiber-Reinforced Structural Foam
AIREX® PXc is a closed-cell, fiber reinforced polymer foam with very high mechanical properties ideally suited as core material for structurally loaded sandwich applications. The sophisticated manu..
Flexural Modulus 0.280 - 4.40 GPa
40.6 - 638 ksi
Average value: 1.10 GPa Grade Count:288
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Copyright © lookpolymers.com All Rights Reserved