Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
flex bar, Injection
0.013 cm/cm
0.013 in/in
disk, Injection
Mechanical Properties Metric English Comments
Hardness, Shore D 42 - 48

@Time 5.00 sec
42 - 48

@Time 0.00139 hour
ASTM D2240
Tensile Strength 40.0 MPa
5800 psi
ASTM D412
Elongation at Break 575 %
575 %
ASTM D412
100% Modulus 0.00900 GPa
1.31 ksi
ASTM D412
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Flexural Modulus 0.0593 GPa
8.60 ksi
ASTM D790
Tear Strength 36.8 kN/m
210 pli
Trouser; ASTM D470
Graves Tear Strength 128 kN/m
730 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 0.70
0.70
CS-17, 1000 g; ASTM D3389 B
Compression Set 35 %

@Temperature 23.0 °C,
Time 79200 sec
35 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
39 %

@Temperature 70.0 °C,
Time 79200 sec
39 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
DSC
Glass Transition Temp, Tg -46.0 °C
-50.8 °F
DSC
Processing Properties Metric English Comments
Rear Barrel Temperature 204 °C
399 °F
Injection
Middle Barrel Temperature 210 °C
410 °F
Injection
Front Barrel Temperature 218 °C
424 °F
Injection
Nozzle Temperature 221 °C
430 °F
Injection
Melt Temperature 221 °C
430 °F
Injection
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Injection Pressure 10000 - 15000 MPa
1.45e+6 - 2.18e+6 psi
Injection
Hold Pressure 5000 - 10000 MPa
725000 - 1.45e+6 psi
Injection
Back Pressure >= 50.0 MPa
>= 7250 psi
Injection
Screw Speed 60 - 100 rpm
60 - 100 rpm
Injection