Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.10 J/cm

@Temperature 23.0 °C
9.55 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Izod Impact, Unnotched 5.10 J/cm

@Temperature -30.0 °C
9.55 ft-lb/in

@Temperature -22.0 °F
ASTM D 4812
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Izod Impact, Unnotched 5.10 J/cm

@Temperature 23.0 °C
9.55 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Izod Impact, Unnotched 5.10 J/cm

@Temperature -30.0 °C
9.55 ft-lb/in

@Temperature -22.0 °F
ASTM D 4812
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Izod Impact, Unnotched 5.10 J/cm

@Temperature -30.0 °C
9.55 ft-lb/in

@Temperature -22.0 °F
ASTM D 4812
SABIC Innovative Plastics Noryl GFN1420V PPE+PS
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Izod Impact, Unnotched 5.10 J/cm

@Temperature 23.0 °C
9.55 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Noryl GFN1420V PPE+PS