Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.10 J/cm @Temperature 23.0 °C |
9.55 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Izod Impact, Unnotched | 5.10 J/cm @Temperature -30.0 °C |
9.55 ft-lb/in @Temperature -22.0 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Izod Impact, Unnotched | 5.10 J/cm @Temperature 23.0 °C |
9.55 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Izod Impact, Unnotched | 5.10 J/cm @Temperature -30.0 °C |
9.55 ft-lb/in @Temperature -22.0 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Izod Impact, Unnotched | 5.10 J/cm @Temperature -30.0 °C |
9.55 ft-lb/in @Temperature -22.0 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Izod Impact, Unnotched | 5.10 J/cm @Temperature 23.0 °C |
9.55 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |