Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.294 J/cm @Thickness 12.7 mm |
0.550 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP842 Paper Base Laminate
(discontinued **) Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0.. |
|||
Izod Impact, Unnotched | 0.294 J/cm @Thickness 12.7 mm |
0.550 ft-lb/in @Thickness 0.500 in |
CW, E-48/50 |
Industrial Laminates/Norplex ES-1 Engraving Stock Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620â€, 0.125â€, and 0.500†|
|||
Izod Impact, Unnotched | 0.294 J/cm @Thickness 12.7 mm |
0.550 ft-lb/in @Thickness 0.500 in |
CW, E-48/50 |
Industrial Laminates/Norplex ES-2 Engraving Stock Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies. |
|||
Izod Impact, Unnotched | 0.294 J/cm @Thickness 12.7 mm |
0.550 ft-lb/in @Thickness 0.500 in |
CW, E-48/50 |
Industrial Laminates/Norplex ES-3 Engraving Stock Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin. |
|||
Izod Impact, Unnotched | 0.294 J/cm @Thickness 12.7 mm |
0.550 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP600 Paper Base Laminate Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is most commonly used for drill entry material in the PCB industry. Thickness Tested: 0.062".. |
|||
Izod Impact, Unnotched | 0.294 J/cm @Thickness 12.7 mm |
0.550 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP602 Paper Base Laminate Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. It is typically hot punched for numerous low voltage, less than 250 volts, electrical applications.Thickne.. |
|||
Izod Impact, Unnotched | 0.294 J/cm @Thickness 12.7 mm |
0.550 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP630 Paper Base Laminate Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500" |