Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.294 J/cm

@Thickness 12.7 mm
0.550 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP842 Paper Base Laminate  (discontinued **)
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0..
Izod Impact, Unnotched 0.294 J/cm

@Thickness 12.7 mm
0.550 ft-lb/in

@Thickness 0.500 in
CW, E-48/50
Industrial Laminates/Norplex ES-1 Engraving Stock
Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620”, 0.125”, and 0.500”
Izod Impact, Unnotched 0.294 J/cm

@Thickness 12.7 mm
0.550 ft-lb/in

@Thickness 0.500 in
CW, E-48/50
Industrial Laminates/Norplex ES-2 Engraving Stock
Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies.
Izod Impact, Unnotched 0.294 J/cm

@Thickness 12.7 mm
0.550 ft-lb/in

@Thickness 0.500 in
CW, E-48/50
Industrial Laminates/Norplex ES-3 Engraving Stock
Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin.
Izod Impact, Unnotched 0.294 J/cm

@Thickness 12.7 mm
0.550 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP600 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is most commonly used for drill entry material in the PCB industry. Thickness Tested: 0.062"..
Izod Impact, Unnotched 0.294 J/cm

@Thickness 12.7 mm
0.550 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP602 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. It is typically hot punched for numerous low voltage, less than 250 volts, electrical applications.Thickne..
Izod Impact, Unnotched 0.294 J/cm

@Thickness 12.7 mm
0.550 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP630 Paper Base Laminate
Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500"