Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.60 GPa @Temperature -40.0 °C |
1250 ksi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |