Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.62 GPa @Temperature 23.0 °C |
1250 ksi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 8.60 GPa @Temperature -40.0 °C |
1250 ksi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 8.62 GPa @Temperature 23.0 °C |
1250 ksi @Temperature 73.4 °F |
50%RH; ASTM D790 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |