Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.60 GPa @Temperature 80.0 °C |
957 ksi @Temperature 176 °F |
Practical Use (Water Absorption 1.25%); ASTM-D790 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 6.60 GPa @Temperature -40.0 °C |
957 ksi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.8%); ASTM-D790 |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |