Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.60 GPa @Temperature 23.0 °C |
522 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 3.60 GPa @Temperature 23.9 °C |
522 ksi @Temperature 75.0 °F |
ASTM D790 |
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide Melidin® 7021 CM is a self-lubricating compression molded polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best fo.. |
|||
Flexural Modulus | 3.60 GPa @Temperature 260 °C |
522 ksi @Temperature 500 °F |
ASTM D790 |
Saint-Gobain Meldin® 7022 CM Compression Molded Graphite Filled Polyimide Melidin® 7022 CM is a compression molded polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin.. |
|||
Flexural Modulus | 3.60 GPa @Temperature -40.0 °C |
522 ksi @Temperature -40.0 °F |
Practical Use (Water Absorption 3.5%); ASTM-D790 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 3.60 GPa @Temperature -40.0 °C |
522 ksi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 3.60 GPa @Temperature 23.0 °C |
522 ksi @Temperature 73.4 °F |
EN ISO 178 |
Ensinger TECASINT™ 2011 Polyimide (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |