Mechanical Properties Metric English Comments
Flexural Modulus 3.20 GPa

@Temperature 80.0 °C
464 ksi

@Temperature 176 °F
Practical Use (Water Absorption 1.7%); ASTM-D790
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.20 GPa

@Temperature 23.0 °C
464 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.20 GPa

@Temperature 80.0 °C
464 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® NB-5550 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.20 GPa

@Temperature 232 °C
464 ksi

@Temperature 450 °F
Autoclave Cured; [90°]16; Wet condition
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form
Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel
Flexural Modulus 3.20 GPa

@Temperature 23.0 °C
464 ksi

@Temperature 73.4 °F
ASTM D790
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT
Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide..
Flexural Modulus 3.20 GPa

@Temperature 23.0 °C
464 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.8%); ASTM-D790
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..