Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.97 GPa @Temperature 23.0 °C |
431 ksi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Flexural Modulus | 2.97 GPa @Temperature 23.0 °C |
431 ksi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |