Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2.97 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.97 GPa

@Temperature 23.0 °C
431 ksi

@Temperature 73.4 °F
ASTM D790
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
Flexural Modulus 2.97 GPa

@Temperature 23.0 °C
431 ksi

@Temperature 73.4 °F
ASTM D790
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer
Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod..