Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 22.1 GPa @Temperature 23.0 °C |
3210 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel |
|||
Flexural Modulus | 22.1 GPa @Temperature 71.0 °C |
3210 ksi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F515; Fiber 75-1/0Information provided by HexCel |