Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 22.1 GPa @Temperature 21.1 °C |
3200 ksi @Temperature 70.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Modulus | 22.1 GPa @Temperature -53.9 °C |
3200 ksi @Temperature -65.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Modulus | 22.1 GPa @Temperature 21.1 °C |
3200 ksi @Temperature 70.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Modulus | 22.1 GPa @Temperature 23.9 °C |
3200 ksi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:.. |
|||
Flexural Modulus | 22.1 GPa @Temperature 149 °C |
3200 ksi @Temperature 300 °F |
0° Direction, Dry; ASTM D790 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Flexural Modulus | 22.1 GPa @Thickness 1.57 mm |
3200 ksi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex P95 Glass Fabric Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested.. |
|||
Flexural Modulus | 22.1 GPa @Temperature 23.0 °C |
3210 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel |
|||
Flexural Modulus | 22.1 GPa @Temperature 71.0 °C |
3210 ksi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F515; Fiber 75-1/0Information provided by HexCel |