Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 32.8 J @Thickness 3.20 mm, Temperature 23.0 °C |
24.2 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
Injection Molded, Peak Energy; ASTM D3763 |
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp.. |
|||
Dart Drop, Total Energy | 32.8 J @Thickness 3.20 mm, Temperature 23.0 °C |
24.2 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
3.39 m/sec, Peak Energy; ASTM D3763 |
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Dart Drop, Total Energy | 32.8 J @Thickness 3.20 mm, Temperature -29.0 °C |
24.2 ft-lb @Thickness 0.126 in, Temperature -20.2 °F |
6.71 m/sec, Peak Energy; ASTM D3763 |
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS) Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions... |