Dart Drop, Total Energy 32.8 J

@Thickness 3.20 mm,
Temperature 23.0 °C
24.2 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
Injection Molded, Peak Energy; ASTM D3763
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp..
Dart Drop, Total Energy 32.8 J

@Thickness 3.20 mm,
Temperature 23.0 °C
24.2 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
3.39 m/sec, Peak Energy; ASTM D3763
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi..
Dart Drop, Total Energy 32.8 J

@Thickness 3.20 mm,
Temperature -29.0 °C
24.2 ft-lb

@Thickness 0.126 in,
Temperature -20.2 °F
6.71 m/sec, Peak Energy; ASTM D3763
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions...