Rupture Strength 41.0 MPa

@Temperature 750 °C,
Time 3.60e+7 sec
5950 psi

@Temperature 1380 °F,
Time 10000 hour
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel
Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr..
Rupture Strength 41.0 MPa

@Temperature 750 °C,
Time 3.60e+7 sec
5950 psi

@Temperature 1380 °F,
Time 10000 hour
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Rupture Strength 41.0 MPa

@Temperature 927 °C,
Time 3.60e+6 sec
5950 psi

@Temperature 1700 °F,
Time 1000 hour
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Rupture Strength 41.0 MPa

@Temperature 760 °C,
Time 360000 sec
5950 psi

@Temperature 1400 °F,
Time 100 hour
Typical Stress-Rupture
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Rupture Strength 41.0 MPa

@Temperature 927 °C,
Time 3.60e+6 sec
5950 psi

@Temperature 1700 °F,
Time 1000 hour
Sheet
Special Metals UDIMET® alloy 188 Cobalt-base Alloy
UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small ..
Rupture Strength 41.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
5950 psi

@Temperature 1470 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 25Cr/20Ni No. HR6
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..
Rupture Strength 41.0 MPa

@Temperature 927 °C,
Time 3.60e+6 sec
5950 psi

@Temperature 1700 °F,
Time 1000 hour
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..