Mechanical Properties Metric English Comments
Rupture Strength 20.0 MPa

@Temperature 850 °C,
Time 3.60e+7 sec
2900 psi

@Temperature 1560 °F,
Time 10000 hour
Outokumpu 353MA® High Temperature Austenitic Stainless Steel
Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but..
Rupture Strength 20.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
2900 psi

@Temperature 1470 °F,
Time 10000 hour
Outokumpu 4841 High Temperature Austenitic Stainless Steel
Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r..
Rupture Strength 20.0 MPa

@Temperature 899 °C,
Time 3.60e+7 sec
2900 psi

@Temperature 1650 °F,
Time 10000 hour
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Rupture Strength 20.0 MPa

@Temperature 899 °C,
Time 3.60e+7 sec
2900 psi

@Temperature 1650 °F,
Time 10000 hour
ATI Allegheny Ludlum 310H Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Rupture Strength 20.0 MPa

@Temperature 899 °C,
Time 3.60e+7 sec
2900 psi

@Temperature 1650 °F,
Time 10000 hour
ATI Allegheny Ludlum 310S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Rupture Strength 20.0 MPa

@Temperature 899 °C,
Time 3.60e+7 sec
2900 psi

@Temperature 1650 °F,
Time 10000 hour
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Rupture Strength 20.0 MPa

@Temperature 950 °C,
Time 3.60e+7 sec
2900 psi

@Temperature 1740 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite Standard Nickel Alloy Castings, No. HR4
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..