Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00390 GPa | 0.566 ksi | ASTM D412 |
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
50% Modulus | 0.00390 GPa | 0.566 ksi | |
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, .. |