Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, Europe, Middle East, Africa and India Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ISO 2781
Maximum Moisture Content 0.10
0.10
Melt Flow 45 - 65 g/10 min

@Load 8.70 kg,
Temperature 190 °C
45 - 65 g/10 min

@Load 19.2 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ISO 868
Tensile Strength at Break 33.0 MPa
4790 psi
ISO 527-3/5/500
Elongation at Break 625 %
625 %
50% Modulus 0.00390 GPa
0.566 ksi
100% Modulus 0.00460 GPa
0.667 ksi
300% Modulus 0.00720 GPa
1.04 ksi
Tear Strength 38.0 kN/m
217 pli
ISO 34B
Abrasion 58
58
[mm<sup>3</sup>]
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Zone 1 180 °C
356 °F
Extrusion
Zone 2 180 °C
356 °F
Extrusion
Zone 3 175 °C
347 °F
Extrusion
Zone 4 175 °C
347 °F
Extrusion
Adapter Temperature 170 °C
338 °F
5, Extrusion
Die Temperature 170 °C
338 °F
6, Extrusion
Roll Temperature 160 °C
320 °F
1, Extrusion
170 °C
338 °F
2, Extrusion
Drying Temperature 90.0 °C
194 °F
Dry Time 3.00 hour
3.00 hour
Dew Point -40.0 - -30.0 °C
-40.0 - -22.0 °F
Copyright © lookpolymers.com All Rights Reserved