Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 750 MPa @Time 3.60e+6 sec |
109000 psi @Time 1000 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Zytel® 103FHSA NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHSA NC010 is a heat stabilized lubricated polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1000 hours | 750 MPa @Time 3.60e+6 sec |
109000 psi @Time 1000 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST801 is an unreinforced super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity r.. |
|||
Tensile Creep Modulus, 1000 hours | 750 MPa @Temperature 23.0 °C |
109000 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |