Polymer Property : Tenacity = 2.50 g/denier Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.221 - 0.441 N/tex
2.50 - 5.00 g/denier
ASTM D2256/ASTM D3822
NatureWorks® Ingeo™ 6201D Fiber Grade PLA
NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically ..
Tenacity 0.221 - 0.441 N/tex
2.50 - 5.00 g/denier
ASTM D2256/ASTM D3822
NatureWorks® Ingeo™ 6202D Fiber Grade PLA
NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically ..
Tenacity 0.221 - 0.441 N/tex
2.50 - 5.00 g/denier
ASTM D2256/ASTM D3822
NatureWorks® Ingeo™ 6204D Fiber Grade PLA
NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically ..
Tenacity 0.221 - 0.353 N/tex
2.50 - 4.00 g/denier
ASTM D2256/ASTM D3822
NatureWorks® Ingeo™ 6751D Fiber Grade PLA
NatureWorks® PLA polymer 6751D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6751D is designed for extrusion into mechanically ..
Tenacity 0.221 - 0.353 N/tex
2.50 - 4.00 g/denier
ASTM D2256/ASTM D3822
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer
Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f..
Tenacity 0.221 N/tex
2.50 g/denier
ASTM D3218
Total PPH M3766 Metallocene Isostatic Polypropylene Polymer, Fiber Grade
M3766 is an isostatic form of polypropylene made via TOTAL proprietary technology.Recommended Applications. M3766 is recommended for melt spun and spun bound fiber applications. However, due to it..