Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.221 - 0.353 N/tex | 2.50 - 4.00 g/denier | ASTM D2256/ASTM D3822 |
NatureWorks® Ingeo™ 6751D Fiber Grade PLA NatureWorks® PLA polymer 6751D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6751D is designed for extrusion into mechanically .. |
|||
Tenacity | 0.221 - 0.353 N/tex | 2.50 - 4.00 g/denier | ASTM D2256/ASTM D3822 |
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f.. |
|||
Tenacity | 0.168 - 0.353 N/tex | 1.90 - 4.00 g/denier | Average value: 0.255 N/tex Grade Count:14 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Tenacity | 0.282 - 0.353 N/tex | 3.20 - 4.00 g/denier | LFL-09 |
Intercontinental Polymers 1180 Bicomponent PP/PET Fiber Type - 3 Denier X 1.5 Inches 40/60 PP Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdenier.. |
|||
Tenacity | 0.282 - 0.353 N/tex | 3.20 - 4.00 g/denier | LFL-09 |
Intercontinental Polymers 1613 Bicomponent PBN/PET Fiber Type - 1.8 Denier X 3.0 Inches 50/50 PBN Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdenie.. |
|||
Tenacity | 0.265 - 0.353 N/tex | 3.00 - 4.00 g/denier | LFL-09 |
Intercontinental Polymers 1631 Bicomponent Polyester/PET Fiber Type - 4 Denier X 2 Inches Semi-crystalline low melt polyester sheath/PET core. Luster: Semi-Dull. Finish: HydrophilicApplications of bicomponent polyester fiber: Absorbent products, FDA-compliant products, non-wovens, fi.. |