Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |