Polymer Property : Heat Seal Strength Initiation Temperature = 105 °C Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm)
LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm)
LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 30 µm)
LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm)
LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm)
LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 25 µm)
LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm)
LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 18 µm)
LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm)
LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm)
LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm)
LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm)
LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 20 µm)
LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm)
LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 30 µm)
LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm)
LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm)
LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 25 µm)
LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 18 µm)
LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side ..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm)
LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side ..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm)
LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side ..
Heat Seal Strength Initiation Temperature 105 - 110 °C
221 - 230 °F
Kinlead
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm)
LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side ..
Heat Seal Strength Initiation Temperature 105 °C
221 °F
Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin
TOTAL Petrochemicals Polypropylene LX5 02-15 is an experimental grade of isostatic polypropylene copolymer produced via TOTAL proprietary metallocene catalyst technology.Benefits. LX5 02-15 produc..
Heat Seal Strength Initiation Temperature 105 °C
221 °F
Total PPR Z9421 Polypropylene, Random Copolymer, Heat Sealable Film Grade
Color/Clarity/Impact. TOTAL Petrochemicals Polypropylene Z9421 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable. The very low melting..
Heat Seal Strength Initiation Temperature 105 °C
221 °F
1 lb/in heat seal strength; 1.0 mil coating onto 50 lb Kraft paper; Dow Method
Dow 722 Low Density Polyethylene (LDPE)
Polyethylene 722 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry foods packaging, snack foods packaging, moist foods pac..
Heat Seal Strength Initiation Temperature 105 °C
221 °F
Sealing Initial Temperature; Braskem® Method
Braskem BF 2021 LDPE Cast Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Films for absorbents and diapers (with HDPE and LLDPE); general purpose. Information provi..
Heat Seal Strength Initiation Temperature 105 °C
221 °F
Sealing Initial Temperature; Braskem® Method
Braskem EB 861 LDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Coextruded films; Shrink films for pallets; general purpose; mulching films. Information p..
Heat Seal Strength Initiation Temperature 105 °C
221 °F
Sealing Initial Temperature; Braskem® Method
Braskem EB 853 LDPE Cast Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Films for absorbents and diapers (with HDPE and LLDPE); general purpose. Information provi..
Heat Seal Strength Initiation Temperature 105 °C
221 °F
Sealing Initial Temperature; Braskem® Method
Braskem EB 861/51 LDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Coextruded films; Shrink films for pallets; general purpose. Information provided by Brask..
Heat Seal Strength Initiation Temperature 105 - 130 °C
221 - 266 °F
Average value: 113 °C Grade Count:56
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..